Tunneling effect in a polymer/carbon nanotube nanocomposite strain sensor N Hu, Y Karube, C Yan, Z Masuda, H Fukunaga Acta materialia 56 (13), 2929-2936, 2008 | 1133 | 2008 |
Investigation on sensitivity of a polymer/carbon nanotube composite strain sensor N Hu, Y Karube, M Arai, T Watanabe, C Yan, Y Li, Y Liu, H Fukunaga Carbon 48 (3), 680-687, 2010 | 834 | 2010 |
A critical review of fused deposition modeling 3D printing technology in manufacturing polylactic acid parts Z Liu, Y Wang, B Wu, C Cui, Y Guo, C Yan The International Journal of Advanced Manufacturing Technology 102, 2877-2889, 2019 | 460 | 2019 |
The electrical properties of polymer nanocomposites with carbon nanotube fillers N Hu, Z Masuda, C Yan, G Yamamoto, H Fukunaga, T Hashida Nanotechnology 19 (21), 215701, 2008 | 430 | 2008 |
Stable Seamless Interfaces and Rapid Ionic Conductivity of Ca–CeO2/LiTFSI/PEO Composite Electrolyte for High‐Rate and High‐Voltage All‐Solid‐State Battery H Chen, D Adekoya, L Hencz, J Ma, S Chen, C Yan, H Zhao, G Cui, ... Advanced Energy Materials 10 (21), 2000049, 2020 | 342 | 2020 |
Recent advances in fabrication and characterization of graphene-polymer nanocomposites DG Galpayage Dona, M Wang, M Liu, N Motta, E Waclawik, C Yan Graphene 1 (2), 30-49, 2012 | 333 | 2012 |
Exploiting a robust biopolymer network binder for an ultrahigh-areal-capacity Li–S battery J Liu, DGD Galpaya, L Yan, M Sun, Z Lin, C Yan, C Liang, S Zhang Energy & Environmental Science 10 (3), 750-755, 2017 | 324 | 2017 |
Clay-supported nanoscale zero-valent iron composite materials for the remediation of contaminated aqueous solutions: a review N Ezzatahmadi, GA Ayoko, GJ Millar, R Speight, C Yan, J Li, S Li, J Zhu, ... Chemical engineering journal 312, 336-350, 2017 | 318 | 2017 |
Atomic resolution of structural changes in elastic crystals of copper(II) acetylacetonate A Worthy, A Grosjean, MC Pfrunder, Y Xu, C Yan, G Edwards, JK Clegg, ... Nature chemistry 10 (1), 65-69, 2018 | 305 | 2018 |
Effect of defects on fracture strength of graphene sheets MC Wang, C Yan, L Ma, N Hu, MW Chen Computational Materials Science 54, 236-239, 2012 | 283 | 2012 |
Dual-functional gum arabic binder for silicon anodes in lithium ion batteries M Ling, Y Xu, H Zhao, X Gu, J Qiu, S Li, M Wu, X Song, C Yan, G Liu, ... Nano Energy 12, 178-185, 2015 | 278 | 2015 |
Interweaving 3D network binder for high‐areal‐capacity Si anode through combined hard and soft polymers T Liu, Q Chu, C Yan, S Zhang, Z Lin, J Lu Advanced Energy Materials 9 (3), 1802645, 2019 | 268 | 2019 |
Polyurethane (PU) scaffolds prepared by solvent casting/particulate leaching (SCPL) combined with centrifugation DC Sin, X Miao, G Liu, F Wei, G Chadwick, C Yan, T Friis Materials Science and Engineering: C 30 (1), 78-85, 2010 | 240 | 2010 |
An advance review of solid-state battery: Challenges, progress and prospects C Li, Z Wang, Z He, Y Li, J Mao, K Dai, C Yan, J Zheng Sustainable Materials and Technologies 29, e00297, 2021 | 228 | 2021 |
Experimental and numerical investigation of microstructure and mechanical behavior of titanium/steel interfaces prepared by explosive welding Q Chu, M Zhang, J Li, C Yan Materials Science and Engineering: A 689, 323-331, 2017 | 228 | 2017 |
Stiffness and strength tailoring of cobalt chromium graded cellular structures for stress-shielding reduction S Limmahakhun, A Oloyede, K Sitthiseripratip, Y Xiao, C Yan Materials & Design 114, 633-641, 2017 | 215 | 2017 |
Preparation of graphene oxide/epoxy nanocomposites with significantly improved mechanical properties D Galpaya, M Wang, G George, N Motta, E Waclawik, C Yan Journal of Applied Physics 116 (5), 2014 | 207 | 2014 |
A mechanically robust self-healing binder for silicon anode in lithium ion batteries H Chen, Z Wu, Z Su, S Chen, C Yan, M Al-Mamun, Y Tang, S Zhang Nano Energy 81, 105654, 2021 | 203 | 2021 |
Pull-out simulations on interfacial properties of carbon nanotube-reinforced polymer nanocomposites Y Li, Y Liu, X Peng, C Yan, S Liu, N Hu Computational Materials Science 50 (6), 1854-1860, 2011 | 171 | 2011 |
3D-printed cellular structures for bone biomimetic implants S Limmahakhun, A Oloyede, K Sitthiseripratip, Y Xiao, C Yan Additive Manufacturing 15, 93-101, 2017 | 166 | 2017 |